Brand: C18150
Chemical composition: Cr0.5%~1.5%, Zr0.06%~0.2%, Cu balance
Elongation rate: ≥ 15
Conductivity: ≥ 80%IACS
Thermal conductivity: 330% W/M, K20 ° C
Compressive strength: ≥ 450
Yield strength:/ Hardness: HRB≥75

Brand: C17200
Chemical composition: Be1.8%~2.2%, Co0.3%~0.6%, Cu balance
Elastic modulus: 128Gpa
Conductivity: 24%IACS
Thermal conductivity: 120%W/M,K20°℃
Tensile strength: 1100Mpa~1500Mpa
yield strength: 950Mpa~1150Mpa
Hardness: HRC36°~42°